جزئیات محصول
نام تجاری: HUAO
شرایط پرداخت و حمل و نقل
Packaging Details: Wooden Case
شرایط پرداخت: پیش از این 100 ٪/ 30 ٪ TT پیش از این ، پرداخت تعادل تحویل.
پایان سطح: |
براق |
مقاومت در برابر ضربه: |
عالی |
مادی: |
سرامیک 95% آلومینا |
مقاومت در برابر شوک حرارتی: |
عالی |
مقاومت شیمیایی: |
عالی |
اندازه: |
130*50*15mm |
قدرت فشاری: |
2000 MPa |
رنگ: |
سفید |
پایان سطح: |
براق |
مقاومت در برابر ضربه: |
عالی |
مادی: |
سرامیک 95% آلومینا |
مقاومت در برابر شوک حرارتی: |
عالی |
مقاومت شیمیایی: |
عالی |
اندازه: |
130*50*15mm |
قدرت فشاری: |
2000 MPa |
رنگ: |
سفید |
Alumina Ceramic Tiles are engineered for durability and longevity in demanding industrial applications. Their exceptional wear resistance maintains integrity in high-traffic and abrasive conditions, reducing maintenance needs and providing long-term cost efficiency.
Featuring outstanding thermal shock resistance, these tiles withstand sudden temperature changes without cracking, ensuring reliable performance in thermally demanding environments.
The standard 130×50×15mm size facilitates easy installation and compatibility with existing structures. With a remarkable temperature resistance up to 1800°C, these tiles outperform other materials in extreme heat conditions.
| Parameter | Value |
|---|---|
| Color | White |
| Material | 95% Alumina Ceramic |
| Surface Finish | Glossy |
| Size | 130×50×15mm |
| Compressive Strength | 2000 MPa |
| Hardness | 9 on Mohs Scale |
| Impact Resistance | High |
| Wear Resistance | High |
| Chemical Resistance | Excellent |
| Temperature Resistance | Up to 1800°C |
When calcining cement clinker in a cement rotary kiln, the temperature inside the kiln reaches 1450 ℃, and the materials (such as limestone and clay) have severe erosion and wear on the kiln lining. Ordinary refractory bricks need to be replaced after 3-6 months, resulting in frequent shutdowns of the rotary kiln. Our alumina ceramic bricks have a fire resistance of 1700 ℃ and 5 times the erosion resistance of ordinary refractory bricks. After being attached to the lining of the high-temperature zone of the rotary kiln, the service life of the kiln lining is extended from 4 months to 1 year, and the continuous operation time of the rotary kiln is extended from 30 days to 90 days. After the use of a certain cement plant, the number of kiln shutdowns for maintenance has been reduced by 4 times per year, resulting in an increase of 50000 tons of cement production and saving 380000 yuan in refractory brick replacement costs, which meets the high-efficiency production needs of the cement industry.